Thermoforming

Effortless thermoforming without any compromises on the strength is a unique feature of Indowud nf. The high ‘content of natural fibres makes sure that the density and dimensional stabilty is uncompromised post thermoforming.

Heating temperature 140 - 170 degrees Celsius
Heating time 1-2 minim of board thickness (for example 18-36 minutes for 18 mm board)
Locking (desired shape) time 5 minutes
Cooling time 1-2 minutesimm of board thickness

NOTE

1. The panel may shrink while heating and
giving a shape.

2. Suggested time may vary depending
onthe design.